XRD Analysis in Front of a Corrosion Crack Tip

  • C. GHEORGHIEŞ "Dunarea de Jos" University of Galati, Romania
  • S. LEVCOVICI "Dunarea de Jos" University of Galati, Romania
  • V. PĂUNOIU "Dunarea de Jos" University of Galati, Romania
  • L. GHEORGHIEŞ "Dunarea de Jos" University of Galati, Romania
  • C. OANCEA "Dunarea de Jos" University of Galati, Romania
  • I. OSTACHE "Dunarea de Jos" University of Galati, Romania
  • P. ALEXANDRU "Dunarea de Jos" University of Galati, Romania
Keywords: stainless steel, structure, corrosion, crack, SEM, XRD

Abstract

During exploitation of the heat exchangers some damages can appear in the contact region between the gaskets and the stainless steel walls. The studies upon the material were performed using SEM microscopy, X-ray diffractometry and the finite element method. The obtained data allow the explanation of the complex damage mechanism of the heat exchanger wall. Following our research, the manufacturing technology of the heat exchangers was changed and this way the rebuts were eliminated. The performed research is based upon physical methods and the damage mechanism of the heat exchanger plates is explained by means of the physical phenomena that appear and develop during working conditions.

Creative Commons License

Downloads

Download data is not yet available.

References

[1]. Gheorghies, 1990, C. Controlul structurii fine a materialelor cu radiatii X, Ed. Tehnica, Bucuresti, p. 272.
[2]. He, S., Jiang, P.X., Xu, Y.J., Shi, R.F., Kim, W.S. and Jackson, J.D., Int. J. Therm. Sci., 2005, vol. 44(6), p. 521-530.
[3]. Satake, S., Kunugi, T., Shehata, A. M. and McEligot, D. M., 2000, Int. J. Heat Fluid Flow, 21, p. 526-534.
[4]. Lours, P., Huchet, L., 2001, Analyse d’avaries de pieces metalliques, Ecole des Mines d’Albi-Carmaux, France.
[5]. Stephen, A. J., 2003, International Journal of Heat and Fluid Flow, vol. 24, Issue 6.
[6]. Kim, W. S., Jackson, J.D., He S. and Li, J., 2004, Journal of Mechanical Engineering Science, vol. 218, p. 1361-1372.
[7]. ***, STAS 3583-87.
[8]. ***, STAS 7657-78.
[9]. Lucan, D., Pirvan, I., Radulescu, M., Fulger, M., Jinescu,G., 1998, Revista de chimie vol. 49, p. 222-226.
[10]. ***, STAS 7114/1991.
[11]. Vukoslavcevic, P., and Wallace, J. M., 2001, 54th Annual Meeting, San Diego, USA, November. Bull., Amer. Phys. Soc., 46 (No. 10), p. 89.
[12]. Gheorghies, C., 2003, The Ann. of Dunarea de Jos Univ. of Galati, Fasc. VIII, Tribology, vol. I, p. 302-312.
Published
2008-05-15
How to Cite
1.
GHEORGHIEŞ C, LEVCOVICI S, PĂUNOIU V, GHEORGHIEŞ L, OANCEA C, OSTACHE I, ALEXANDRU P. XRD Analysis in Front of a Corrosion Crack Tip. The Annals of “Dunarea de Jos” University of Galati. Fascicle IX, Metallurgy and Materials Science [Internet]. 15May2008 [cited 26Dec.2024];31(1):37-6. Available from: https://gup.ugal.ro/ugaljournals/index.php/mms/article/view/3121
Section
Articles

Most read articles by the same author(s)